Dissimilar laser welding of HfTaTi refractory medium-entropy alloy to low-entropy Ni-based superalloy
Hong Lei
,
Han Zhang
,
Xinlei Li
,
Hong Lei
,
Han Zhang
,
Xinlei Li
,
Zhongyang Wan
,
Hao Wang
,
Yao Xie
,
Ning Guo
,
Shengfeng Guo
2025
Journal of Materials Research and Technology
0 citations